Target Used in Skid Test at LASL

The target consists of a 2x2 inches, 10 gage steel plate coated with a thin layer of epoxy resin, sprinkling it with 30-mesh (max) sand, and curing. The plate rests on a rectangular steel pad 4.5 inches thick, as shown in Fig 6 [Pg.324]

The hemispherical drop charge, ca 10-inches in diam, consists of 9-lb inert core and 10-lb of expl. Results of test are reported in terms of the 50% height (measured in feet vertically from center of target) by up and down technique, using 15 to 20 drops for each expl sample [Pg.324]

90/10-PBX 75/25-CycIotol 75/25-Octol Octol +1% Wax Comp A Comp B 5.5 150 75 150 150 A small partial expln was obtd at 30 ft [Pg.324]

55c) A.I. Gol binder, Laboratornyiye Raboty po Teorii Vzryvchatykh Veshchestv (Laboratory Proceedings on Theory of Explosives), Razvuzizdat, Moscow (1963) [Pg.324]

55d) J.N. Ayres, Explosive Properties from Small Gap Test Measurements , Discussion at ERDE, Waltham Abbey, England, Oct 4, 19 3 [Pg.324]