Tamped density g/L DIN ISO 787/11 similar to bulk density however, void volume is reduced by tamping... [Pg.165]

Table 5.9. Maximum packing volume fraction, ( )m, of some fillers calculated by dividing tamped density by specific density of filler... Table 5.9. Maximum packing volume fraction, ( )m, of some fillers calculated by dividing tamped density by specific density of filler...
Tamped Density and Tamped Volume (ISO 787, Part II). The tamped density is the ratio of mass to volume, while the tamped volume is the ratio of volume to mass after tamping under specified conditions. These quantities provide information about the volume requirements of the products. [Pg.153]

Pour density, g/L Tamped density, g/L ASTM D1513... [Pg.976]

In a mote recent formula, cornstarch is replaced bv Guar vum and Engine Oil hy Process Oil Properties of MVD (prior to replacement of cornstarch by Guar gum and use of "Process Oil ) Buff-colored plastic, tamped by Hall Packer machine in the same size cartridges as for LVD at density l.T, it remains plastic to as low as —70°F. Biisance by 200 Gram Bomb - 52.6g sand crushed v 4ft.f) for TNT... [Pg.506]

Detonation Rate — 6000 to 6600 m/sec or 20000 ft/sec for machine-tamped, unconfined cartridges at density 1.1... [Pg.506]

Detonation Rate — 4397m/sec or l4400ft/sec for hand-tamped at density 0,9 unconfined cartridge Explosion Temperature — ignites in 5secs at 480°C Friction Sensitivity — unaffected by steel or fiber shoe... [Pg.507]

Expressions QeV0 and 425Qe take no consideration of the velocity of detonation, a very important factor in the kind of expl action, and one which is very considerably affected by the physical condition of the expl, its aggregate state, density, crystal form and granulation, as well as by extreme conditions of detonation, such as the initiating impulse, confinement and tamping (Ref 2, p 153)... [Pg.739]

Properties of Composition C-4. It is a light -brown soft putty-like plastic explosive which can be hand-tamped to a density of 1.58 - 1.60 g/cc. Its brisance by sand test is 116% of TNT and by plate dent test, method B 115% (for unconfined hand-tamped material at d 1.60) detonation rate at RT, 8040m/sec, for unconfined, hand -tamped chge,diam 1, r d 1.59 Ditto - for sample kept at -54° for 16hrs 7020m/sec at d 1.36, vs 7040m/sec for sample at +21° explosion temperature - 290° in 5secs exudation - none at 77° friction pendulum test - unaffected by... [Pg.268]


See other pages where Tamped density is mentioned: [Pg.487]    [Pg.549]    [Pg.487]    [Pg.549]    [Pg.134]    [Pg.148]    [Pg.265]    [Pg.210]    [Pg.56]    [Pg.152]    [Pg.392]    [Pg.392]    [Pg.393]    [Pg.393]    [Pg.397]    [Pg.398]    [Pg.414]    [Pg.141]    [Pg.62]    [Pg.63]    [Pg.487]    [Pg.549]    [Pg.487]    [Pg.549]    [Pg.134]    [Pg.148]    [Pg.265]    [Pg.210]    [Pg.56]    [Pg.152]    [Pg.392]    [Pg.392]    [Pg.393]    [Pg.393]    [Pg.397]    [Pg.398]    [Pg.414]    [Pg.141]    [Pg.62]    [Pg.63]    [Pg.502]    [Pg.549]    [Pg.629]    [Pg.361]    [Pg.33]    [Pg.427]    [Pg.428]    [Pg.282]    [Pg.780]    [Pg.54]    [Pg.502]    [Pg.549]    [Pg.18]    [Pg.202]    [Pg.504]    [Pg.505]    [Pg.195]    [Pg.280]    [Pg.366]    [Pg.198]   