As reported the aged sisal fiber composites exhibited better mechanical properties than the composites with fresh fibers. Although the aging of other fibers is seldom reported, it could be of great interest to investigate the effect of aging on the properties of fibers as well as their composites. [Pg.394]

Applications of Sisal Fiber Composites in Building Materials. 638... [Pg.590]

Sisal Fiber Composition, Structure and Properties 22.3.1 Composition... [Pg.600]

The impact strength of methyl-methacrylate (MMA)-grafted (5%) sisal fiber composites was found to be 158.29 J/m. However, composites produced from 10% MMA grafted sisal fiber showed high tensile strength, flexural strength, and impact strength of 7%, 13.3%, and 2.7%, respectively [36,37]. In fact, an increase in MMA... [Pg.627]

Properties of randomly orientation of sisal fiber composites are shown in parentheses) PP Polypropylene PS Polystyrene... [Pg.632]

Table 22.13 Tensile properties of maleic anhydride treated sisal fiber composite... Table 22.13 Tensile properties of maleic anhydride treated sisal fiber composite...
Fig. 22.7 Flow chart for development of Sisal fiber composites... Fig. 22.7 Flow chart for development of Sisal fiber composites...
S. Varghese, B. Kuriakose, S. Thomas, and A.T. Koshy, Studies on natural rubbershort sisal fiber composites. Indian J. Nat. Rubber Res. 4, 55 (1991). [Pg.549]

Ramires E C and Frollini E (2012), Tannin-phenolic resins Synthesis, characterization, and application as matrix in biobased composites reinforced with sisal fibers . Composites Part B, 43(7), 2851-2860. [Pg.41]

Besides being used as a dispersed component in polymer blends, TPS was also used as a matrix polymer and was reinforced by natural fibers. TPS/sisal fiber composite prepared by compression molding exhibited improved tensile strength. The strength increased from 4 MPa (neat TPS) to 8 MPa at 10% fiber content [17] Ma et al. [18] prepared TPS/winceyette fiber composite by extrusion. The composite exhibited a tensile strength of 15 MPa at 20% fiber content. [Pg.129]

Nair, K.C.M. and Thomas, S. (2003) Effect of interface modification on the mechanical properties of polystyrene-sisal fiber composites. Polym. Compos., 24, 332-343. [Pg.173]

Nair KCB, Thomas S. 2003. Effect of Interface Modification on the Mechanical Properties of Polystyrene-Sisal Fiber Composites. Polym Composite 24(3) 332-343. [Pg.290]


See other pages where Sisal fiber composites is mentioned: [Pg.72]    [Pg.590]    [Pg.603]    [Pg.604]    [Pg.629]    [Pg.631]    [Pg.636]    [Pg.644]    [Pg.651]    [Pg.652]    [Pg.535]    [Pg.72]    [Pg.235]    [Pg.265]    [Pg.150]   
See also in sourсe #XX -- [ Pg.638 , Pg.639 , Pg.640 , Pg.641 , Pg.642 , Pg.643 ]




SEARCH



Biobased Composites of Sisal Fiber Reinforced Polypropylene

Reinforced polymer composites tensile properties, sisal fiber

Sisal -coir hybrid fiber-reinforced composites