Wei, R. P., and Brazill, R. L., An Assessment of A-C and D-C Potential Systems for Monitoring Fatigue Crack Growth, in Fatigue Crack Growth Measurement and Data Analysis, ASTM STP 738, S. J. Hudak, Jr., and R. J. Bucci, eds., American Society for Testing and Materials, Philadelphia, PA (1981), 103-119. [Pg.214]

H. Nakajima, T. Shoji, M. Kikuchi, H. Nitsuma, M. Shindo, Detecting acoustic emission during cyclic crack growth in simulated BWR environments, in S.J. Hudak, R.J. Bucci (Eds.), Fatigue Crack Growth Measurement and Data Analysis, ASTM STP 738, ASTM International, West Conshohocken, PA, 1981, pp. 139—162. [Pg.446]

Fatigue Crack Growth Measurement and Data Analysis, ASTM STP 738, S. J. Hudak and R. J. Bucci, Eds., ASTM International, West Conshohocken, PA, 1981. [Pg.320]

Wachnicki, C. R., Radon, J.C. Fatigue crack growth measurement in a CSM composite using compliance and Moire techniques. Composites, 15 (1984) 3, p.211-216... [Pg.1352]

ASTM E647-93, "Measurement of Fatigue Crack Growth Rates," Annual Book of ASTM Standards, ASTM Puhhcations, Philadelphia, 1993. [Pg.550]

Special requirements for fatigue testing in aqueous environments are addressed in the Annexe to ASTM E647 1986a Standard Test Method for Measurement of Fatigue Crack Growth Rates . [Pg.1054]

Test method for measurement of fatigue crack growth rates... [Pg.1100]

Superior fatigue behaviour, as measured by the fatigue crack growth rate. [Pg.841]

Now the measured value of KIc or GIc is dependent upon the sharpness of the crack employed and an essential requirement of fracture mechanics testing is that a "naturally sharp crack is used for the experimental determination of K,c or G C. If a relatively blunt crack is used, an optimistically high value of KIc or G,c may be recorded. Suitable techniques include slow, controlled pressure applied to a razor blade, possibly having pre-cooled the specimen in liquid nitrogen and fatigue crack growth. [Pg.49]

A list of alloys for which fatigue crack growth rates were measured is shown in Table I. Included are the material forms, chemical analyses heat treatments, and specimen orientations, according to the ASTM Method E 399-74 notation [% One of the Ti-5Al-2.5Sn alloys contained too much hydrogen (173 ppm) to qualify as an extra-low-interstitial (ELI) grade this material is referred to in the text as a low-interstitial alloy. The compact specimen geometry was chosen because it is standardized and much experience has been accumulated with it. Constant-load... [Pg.82]


See other pages where Fatigue crack growth measurement is mentioned: [Pg.177]    [Pg.177]    [Pg.1288]    [Pg.1295]    [Pg.1298]    [Pg.1300]    [Pg.1308]    [Pg.1309]    [Pg.1322]    [Pg.121]    [Pg.157]    [Pg.174]    [Pg.146]    [Pg.150]    [Pg.153]    [Pg.74]    [Pg.190]    [Pg.204]    [Pg.173]    [Pg.161]    [Pg.428]    [Pg.429]    [Pg.435]    [Pg.103]    [Pg.104]    [Pg.118]    [Pg.169]    [Pg.183]    [Pg.91]    [Pg.293]    [Pg.542]    [Pg.547]    [Pg.548]    [Pg.242]    [Pg.315]    [Pg.481]    [Pg.493]    [Pg.83]   


SEARCH



Crack growth

Crack growth measurements

Crack measurements

Cracks crack growth

Cracks fatigue cracking

Fatigue cracking

Fatigue cracks

Fatigue growth

Fatigue measurement

Growth measurements

© 2024 chempedia.info