Coatings weatherability

Bimodal PE s (LCB = 0.01- 3 > 7) was lightly crosslinked. The PE-1 was prepared in the hrst reactor, and PE-2 was prepared in the presence of 15 - 65 wt% of PE-1 in the second reactor. The reaction could be carried out in the slurry, solution, or gas phase. blends (p < 885 kg/m ) were used for wrre/cable coating, weather-stripping, seals, foamed articles with closed, open or mixed cells, containers, medical appliances, drapes and coverings, hbers, tapes, tubes, pipes and hoses, bellows, boots, gaiters, footwear, etc. Cree etal, 1998... [Pg.52]

Paints and coatings Weathering, disposal Consumers, general population Dermal, inhalation or ingestion... [Pg.687]

Weathering without back coating Weathering with back coating (Fig. 20)... [Pg.715]

Biphenylcarboxaldehyde Chlorodiphenyl (54% Cl) 2-Ethylhexyl methacrylate Maleic acid/acrylic acid copolymer Maleic acid/olefin copolymer, sodium salt paints/coatings, UV light-resistant Polyvinylidene fluoride resin paints/coatings, weathering-resistant Polyvinylidene fluoride resin pallet wrapping Polyethylene, low-density palliative, skin care Aloe... [Pg.5503]

With reference to performance of scribed coated panels, rate of deterioration of weathering steel substrate was lesser than mild steel substrate as per EIS. Deterioration of coated panels was highest at PI for both steels, and also higher for mild steels at P2 and P3 as found by EIS. Presence of SO2 helped to prevent deterioration of coated weathering steels at these sites. [Pg.142]

Keywords Interlayer adhesion loss Epoxy coatings Weathering Erosion mechanism UV absorber Humidity Water Crosslinking Network degradation Oxygen diffusion and solubility Photoproducts Oxidation zone Rain Lag time UV radiation degradation... [Pg.185]

Q-UV test, which is the decrease in gloss at 20 and 60 after exposure at UV light and humidity for a week, indicates that vernonia oil improves the coatings weatherability. [Pg.88]

Vinyl fluoride (fluoroethene), is manufactured from the cataly2ed addition of hydrogen fluoride to acetylene. It is used to prepare poly(vinyl fluoride) which has found use in highly weather-resistant films (Tedlar film, Du Pont). Poly(vinyhdene fluoride) also is used in weather-resistant coatings (see Eluorine compounds, organic). The monomer can be prepared from acetylene, hydrogen fluoride, and chlorine but other nonacetylenic routes are available. [Pg.393]


See other pages where Coatings weatherability is mentioned: [Pg.761]    [Pg.489]    [Pg.131]    [Pg.310]    [Pg.271]    [Pg.140]    [Pg.518]    [Pg.137]    [Pg.8741]    [Pg.185]    [Pg.191]    [Pg.161]    [Pg.73]    [Pg.111]    [Pg.185]    [Pg.254]    [Pg.918]    [Pg.761]    [Pg.489]    [Pg.131]    [Pg.310]    [Pg.271]    [Pg.140]    [Pg.518]    [Pg.137]    [Pg.8741]    [Pg.185]    [Pg.191]    [Pg.161]    [Pg.73]    [Pg.111]    [Pg.185]    [Pg.254]    [Pg.918]    [Pg.169]    [Pg.203]    [Pg.285]    [Pg.285]    [Pg.371]    [Pg.389]    [Pg.389]    [Pg.330]    [Pg.375]    [Pg.545]    [Pg.549]    [Pg.551]    [Pg.201]    [Pg.70]    [Pg.268]    [Pg.271]    [Pg.545]    [Pg.494]    [Pg.494]    [Pg.5]    [Pg.9]    [Pg.14]    [Pg.16]    [Pg.23]    [Pg.209]   
See also in sourсe #XX -- [ Pg.243 , Pg.244 ]