In the following sections, a brief chronology of the development of this process is presented the materials, equipment, and basic operations relating to the resin-bead loading and calcination method of producing sized curium-americium oxide microspheres at TRU are described and typical production data are presented. [Pg.173]

Figure L Curium-americium oxide microsphere production by Dowex 50W-X8 resin-bead loading and calcination... Figure L Curium-americium oxide microsphere production by Dowex 50W-X8 resin-bead loading and calcination...
The resin is then allowed to dry for 10 minutes, while the pump continues to pull air through the resin, before the column is removed to the calcining furnace. Raffinate batches from the individual loading runs are analyzed for 44Cm and usually can be discarded to waste. [Pg.178]

Resin-bead loading and calcination techniques have been used to produce all curium and americium oxide feed material... [Pg.181]


See other pages where Resin loading calcination is mentioned: [Pg.143]    [Pg.143]    [Pg.496]    [Pg.129]    [Pg.172]    [Pg.173]    [Pg.173]    [Pg.178]    [Pg.58]    [Pg.247]    [Pg.220]    [Pg.73]    [Pg.700]    [Pg.458]    [Pg.372]   