Superalloys are usually defined as heat- and oxidation-resistant alloys specially developed for servicing at elevated temperatures under both oxidizing atmosphere and severe mechanical stresses. Three main classes of superaUoys are distinguished  [Pg.145]

NB For stellite alloys the Young s or elastic modulus is between 180 and 249 MPa the bulk or compression modulus is between 152 and 296 MPa the Coulomb s or shear modulus is between 90 and 97 MPa. [Pg.147]