Table 8. Materials Properties of Oxide Dispersion Strengthened Superalloys ... Table 8. Materials Properties of Oxide Dispersion Strengthened Superalloys ...
Arzt, E. Singer, R. F. The effect of grain shape on stress rupture of the oxide dispersion strengthened superalloy INCONEL M A 6000. Proc. of the Seven Spring Conference on Superalloys, The Metallurgical Society of AIME, (1984), pp. 367-376. [Pg.184]

Reinforcement by a fine, homogeneous dispersion of second-phase nanoscale particles is an effective way to achieve strengthening and stability. Oxide dispersion strengthened (ODS) superalloys (Ni-base alloys such as... [Pg.56]

Nazmy, A. Rydstad, H. Process for increasing the oxidation and corrosion resistance of a component made of a dispersion strengthened superalloy by a surface treatment. US Patent, No. 4,909,859 (1990). [Pg.183]


See other pages where Oxide-dispersion strengthened superalloys is mentioned: [Pg.129]    [Pg.17]    [Pg.12]    [Pg.172]    [Pg.257]    [Pg.130]    [Pg.48]    [Pg.746]    [Pg.443]    [Pg.443]    [Pg.212]    [Pg.934]    [Pg.804]    [Pg.199]    [Pg.145]   