Neat CF PEEK examples of tensile strength retention versus temperature C

For long-term heat ageing, property retention depends on the property and grades considered, notably the heat stabilizers used. Impact strength and elongation at break are especially heat-sensitive characteristics. [Pg.560]

Half-lives of specific PEEK grades based on tensile strength are  [Pg.560]

The behaviour at low temperatures is good, depending on the grades and the mechanical constraints experienced. [Pg.560]

Generally, notched Izod impact strengths slowly decrease between room temperature and -40°C retaining, for example, 80-85% of the original value. [Pg.560]


Figure 4.105. Neat CF PEEK examples of tensile strength retention (%) versus temperature (°C)... Figure 4.105. Neat CF PEEK examples of tensile strength retention (%) versus temperature (°C)...



SEARCH



C versus

CF/PEEK

Neatness

PEEK

Retention of

Retention of tensile strength

Retention temperature

Temperature Tensile strength

Temperature strength

Tensil strength

© 2024 chempedia.info