The rubber used was the EPDM compound described in Table 3.2 with 2% peroxide. The Monsanto 2000 E MDR is used under isothermal conditions, while the simulation is done by calculation. The thickness of the sample is taken as equal to 0.2 cm. A calorimeter C 80 was used in scanning mode with a heating rate of 0.2°C/min and a sample of around 6 g. [Pg.69]

The characteristics of cure and of heat transfer are shown in Table 3.7. [Pg.69]

In scanning mode of the MDR, the temperature of the dies and the rubber starts at room temperature (25°C) and increases constantly with time. [Pg.69]