Big Chemical Encyclopedia

Chemical substances, components, reactions, process design ...

Articles Figures Tables About

Intergranular corrosion cast stainless steels

Fig. 19.19 Intergranular corrosion plot for a sensitised cast CF-S stainless steel (0 08 7o C max., 8-11% Ni, 18-21% Cr) in H2 SO4 at 40°C as a function of potential and concentration of acid (after France and Greene )... Fig. 19.19 Intergranular corrosion plot for a sensitised cast CF-S stainless steel (0 08 7o C max., 8-11% Ni, 18-21% Cr) in H2 SO4 at 40°C as a function of potential and concentration of acid (after France and Greene )...
Intergranular corrosion occurs in stainless steels and alloys based on nickel, aluminium, magnesium, copper and cast zinc. In the following sections we shall look at the three former groups in some detail. [Pg.132]

Intergranular Stress Corrosion Cracking Resistance of Austenitic Stainless Steel Castings... [Pg.75]

C. McCaul. 1991. Evaluation of intergranular corrosion susceptibility in as as-welded high alloy austenitic stainless steel casting, British Corrosion Journal, December. [Pg.233]


See other pages where Intergranular corrosion cast stainless steels is mentioned: [Pg.350]    [Pg.279]    [Pg.45]    [Pg.1573]    [Pg.350]    [Pg.322]    [Pg.176]    [Pg.381]    [Pg.78]    [Pg.304]    [Pg.54]    [Pg.248]    [Pg.933]   
See also in sourсe #XX -- [ Pg.350 ]




SEARCH



Cast stainless steels

Cast steel

Castings intergranular corrosion

Intergranular

Intergranular corrosion

Intergranular corrosion stainless steels

Stainless steels cast, corrosion

Stainless steels corrosion

Steel corrosion

© 2024 chempedia.info