These anaerobic adhesives fill all surface irregularities and tolerance gaps and effectively seal clearances up to 0.76 mm. They can be applied by high-speed applications in moving production lines. The cured film has excellent chemical resistance to most liquids and gases within an operating temperature range of -54°C to 232°C. [Pg.68]

Figure 2.19 Effect of temperature on the shear strength of conventional and highly cross-linked anaerobic adhesives. The poorer performance of the conventional version as measured on a standard collar and pin assembly (MoD specification DTD 5628) is quite marked. Figure 2.19 Effect of temperature on the shear strength of conventional and highly cross-linked anaerobic adhesives. The poorer performance of the conventional version as measured on a standard collar and pin assembly (MoD specification DTD 5628) is quite marked.
Increasing the temperature of components assembled with an anaerobic adhesive has three different and quite distinct effects ... [Pg.78]

Fig. 7.22. Effect of temperature on joint strength of anaerobic adhesives. Fig. 7.22. Effect of temperature on joint strength of anaerobic adhesives.

See other pages where Temperature effects anaerobic adhesives is mentioned: [Pg.483]    [Pg.2]    [Pg.454]    [Pg.985]   