Above 370°C, carbon-carbon composites readily oxidize in air, [Pg.573]

Initially, the fiber matrix interface is attacked, resulting in delamination cracking between plies, but as the temperature increases, more severe oxidation attack occurs within the [Pg.573]

Use of inhibitors and sealants to block active sites internally and stifle the rate of oxidation [Pg.574]

Apply a barrier coating to form a protective outside layer, preventing O2 moving inwards and carbon moving out. [Pg.574]