Charge all solvents and 10% of the premixed monomers and 10% of initiator to the reactor with stirring. [Pg.93]

Heat to 80°C - the polymerisation is exothermic - so control the temperature with cooling as necessary to below 10(f C. [Pg.93]

When the initial exotherm is complete add the remaining monomers and initiator as a premix over a three hour period at 90-10(f C. [Pg.93]

Sample for non-volatile content, if below 50% continue heating under reflux, possibly with the addition of a booster shot of peroxide until non-volatile content reaches 50%. [Pg.93]

Cool and discharge through a suitable sized filter. [Pg.93]


See other pages where Preparation of a Thermoplastic Acrylic Resin in Solution is mentioned: [Pg.93]   


SEARCH



A- acrylate

Acrylate resin

Acrylates Acrylic resins

Acrylates preparation

Acrylic resins

Preparation of solutions

Resin preparation

Resin solutions

Solution acrylic resins

Solution preparing

Thermoplastic resin

Thermoplastic solution acrylic resins

© 2024 chempedia.info