Peel Strength of Al-Plasma Copolymer-PP Systems

In the case of allyl alcohol-ethylene plasma copolymers, the maximum adhesion (650 N m ) was measured at 27-29 OH per 100 C atoms. Therewith, this copolymer exhibits a significantly higher peel strength than the aUyl alcohol homopolymer (85 N m ). Thus, the above ranking of the adhesion-promoting [Pg.277]

Functional group Peel strength [N Concentration Type of failure Location [Pg.277]

COOH groups produce the highest peel strength at A1 (see Fig. 18.7 and Table 18.4). In both cases of deposition of acryhc acid-ethylene or -butadiene [Pg.278]

Functional Concentration Strength [N m ] Type of failure Location [Pg.278]

NH2 OH COOH 12-18 NH2/IOOC 27-29 OH/100 C 8-24 COOH/IOOC 10-30 600-620 650 interfacial interfacial cohesive plasma polymer-PP plasma polymer-PP inside PP [Pg.278]


See other pages where Peel Strength of Al-Plasma Copolymer-PP Systems is mentioned: [Pg.277]   