Big Chemical Encyclopedia

Chemical substances, components, reactions, process design ...

Articles Figures Tables About

PA 12 examples of tensile strength retention versus temperature C

For long-term heat ageing, property retention depends on the property and grades considered, notably the heat stabilizers used. Characteristics such as elongation at break and impact strength are especially heat sensitive. [Pg.392]

At low temperatures, general-purpose grades generally have a brittle point of -70°C down to -120°C. [Pg.392]

These results relate to some grades only and cannot be generalized. [Pg.392]

Polyamides 11 and 12 are translucent to opaque according to the thickness and the grade. [Pg.392]


Figure 4.59. PA 12 examples of tensile strength retention (%) versus temperature (°C)... Figure 4.59. PA 12 examples of tensile strength retention (%) versus temperature (°C)...