8 Oxygen-Enhanced Crack Growth in Nickel-Based Superalloys [Pg.143]

24 and 8.25) in that the growth rates in oxygen were nearly 10 times faster than those in argon at 973 K (see Fig. 8.24) ie., with an environmental sensitivity factor that is well above one time to ten times anticipated from the literature data [22]. [Pg.145]


Huang, Z. F., Oxygen Enhanced Crack Growth in Nickel-based Superalloys, Ph.D. Dissertation, Lehigh University (2002). [Pg.157]