Apart from its use in decoy flares, MTV is also used in propellant igniters, and therefore, MTV crumb obtained from shock gel process is extruded in small round or cruciform strands of 2.3-2.4mm diameter. The extrusion is carried out at 121 °C, 4 MPa for round and 8.3 MPa for cruciform strands. Finally, the strand is cut with guillotine type cutter or band saw into length of 3.8-5.8 mm [29, 30]. [Pg.289]

Hazards Posed by Loose In-Process MTV Crumb and TNT Equivalent 321... [Pg.321]

Figure 18.2 Manual transfer of MTV composition crumb in a vacuum oven at Space Ordnance Systems, Canyon, CA, USA in 1980s. Safety note standard protective clothing has changed since. Operations require grounding of the operator and Nomex-type overall with balaclava and additional faceshield. Figure 18.2 Manual transfer of MTV composition crumb in a vacuum oven at Space Ordnance Systems, Canyon, CA, USA in 1980s. Safety note standard protective clothing has changed since. Operations require grounding of the operator and Nomex-type overall with balaclava and additional faceshield.

See other pages where MTV, crumb is mentioned: [Pg.276]    [Pg.286]    [Pg.321]    [Pg.276]    [Pg.286]    [Pg.321]   
See also in sourсe #XX -- [ Pg.274 , Pg.276 , Pg.286 , Pg.289 , Pg.321 ]




SEARCH



Crumb

Hazards Posed by Loose In-Process MTV Crumb and TNT Equivalent

© 2024 chempedia.info