Linear polycarbonate homopolymer

Tensile Yield Stresses of Cast Films. At room temperature all of the BPFC-DMS polymers investigated (with one exception) reached their yield stresses before fracturing. BPF polycarbonate on the other hand is brittle, breaking at about 11,000 psi. Traces of residual chloroform make the homopolymer ductile however the yield stress decreased linearly with chloroform content. Extrapolation of these results to a dry polymer gives a yield stress of 14,000 psi. [Pg.325]