In this respect it should have a sufficiently high viscosity at the mixing temperature for the imposition of shear stress on particle clusters under the influence of machine-imposed shear rates. Conditions of polymer-ceramic wetting may be desirable for stability of the dispersion but the long time required for establishment of the equilibrium contact angle of a high [Pg.231]

Confer fluidity on the powder sufficient for complete filling of the [Pg.231]

Confer adequate strength to the body during ejection fron the mould, [Pg.232]

Distortion during ejection m2iy be caused by low yield stress in the solidified body and is avoided by employing semicrystalline polymers or waxes or species with a glass transition temperature above ambient. [Pg.232]

It is important for high performance ceramic applications that the ash content of the polymer blend should be low in silicates and alkali metals. For moulding of non-carbide ceramics it is desirable to have a low residual carbon content. [Pg.232]