Cast stainless steels, intergranular

Fig. 19.19 Intergranular corrosion plot for a sensitised cast CF-S stainless steel (0 08 7o C max., 8-11% Ni, 18-21% Cr) in H2 SO4 at 40°C as a function of potential and concentration of acid (after France and Greene )... Fig. 19.19 Intergranular corrosion plot for a sensitised cast CF-S stainless steel (0 08 7o C max., 8-11% Ni, 18-21% Cr) in H2 SO4 at 40°C as a function of potential and concentration of acid (after France and Greene )...
Intergranular corrosion occurs in stainless steels and alloys based on nickel, aluminium, magnesium, copper and cast zinc. In the following sections we shall look at the three former groups in some detail. [Pg.132]

Intergranular Stress Corrosion Cracking Resistance of Austenitic Stainless Steel Castings... [Pg.75]

C. McCaul. 1991. Evaluation of intergranular corrosion susceptibility in as as-welded high alloy austenitic stainless steel casting, British Corrosion Journal, December. [Pg.233]


See other pages where Cast stainless steels, intergranular is mentioned: [Pg.350]    [Pg.279]    [Pg.45]    [Pg.1573]    [Pg.350]    [Pg.322]    [Pg.176]    [Pg.244]    [Pg.381]    [Pg.78]    [Pg.304]    [Pg.54]    [Pg.458]    [Pg.248]    [Pg.933]   