Big Chemical Encyclopedia

Chemical substances, components, reactions, process design ...

Articles Figures Tables About

Preparation of Composite Specimen from Wet Resins

A matched metal mold must be carefully ground from hardened steel and the finished dimensions carefully checked. The mold, when new, should be coated with silicone grease and baked for 24 h at 200°C, to acquire a patina with an improved release. All assembly set screws and their sockets should be smeared with silicone grease to prevent resin penetration [Pg.690]

The number of tows required when making a 60% composite bar would be  [Pg.692]


See other pages where Preparation of Composite Specimen from Wet Resins is mentioned: [Pg.690]   