Porous Silicon Nitride Through Sinter-Forging

Porous Silicon Nitride Through Sinter-Forging [Pg.374]

The elastic modulus, measured using the pulse echo method, was about 180 GPa, and the fracture strength determined by the three-point flexure test was about 800 MPa in the grain-alignment direction. This strength, which is relatively high for the large porosity of 25%, is almost equivalent to that of commercially available [Pg.374]


Porous Silicon Nitride Through Sinter-Forging... [Pg.374]

Figure 8.26 Fracture surfaces of porous silicon nitride with fine fibrous grain alignment fabricated through a sinter-forging technique. The porosity is 24%. Illustration courtesy of Naoki Kondo et al. Figure 8.26 Fracture surfaces of porous silicon nitride with fine fibrous grain alignment fabricated through a sinter-forging technique. The porosity is 24%. Illustration courtesy of Naoki Kondo et al.

See other pages where Porous Silicon Nitride Through Sinter-Forging is mentioned: [Pg.374]   