Polyester polymer concrete shrinkage

High-temperature cement formulations are basically polymer concrete. Mainly unsaturated polyesters or vinyl ester resins with allylphthalate as vinyl monomer are in use [927]. Cming is achieved with peroxides, which decompose sufficiently fast at temperamres between 120° and 200° C. Polymer concrete requires additional materials, which compensate shrinkage. [Pg.132]

The vinyl ester resins have lower shrinkage and are generally less rigid than many of the polyester resins. Vinyl ester novolac is a premium vinyl ester resin. Any of the vinyl ester resins can be formulated to produce a polymer concrete that will be capable of resisting normal atmospheric pollution. [Pg.177]


See other pages where Polyester polymer concrete shrinkage is mentioned: [Pg.132]    [Pg.19]    [Pg.41]    [Pg.9]    [Pg.216]    [Pg.364]    [Pg.208]    [Pg.22]    [Pg.28]    [Pg.138]   
See also in sourсe #XX -- [ Pg.19 ]




SEARCH



Concrete shrinkage

Concretes polyester

Polyester polymer concrete

Polymer polyesters

Shrinkage

© 2024 chempedia.info