Percent elongation at failure

Note Alloy was annealed at 815 °C (1500 °F) for 30 min, air cooled. Ultimate tensile strength was (sheet) 896 MPa (130 ksi) and (bar) 930 MPa (135 ksi). (a) Ruptured in time indicated, (b) Percent elongation at failure. Source RMI data, reported in Engineering Properties of Titanium Alloys, TML Report 92, Battelle Memorial Institute, 1969... [Pg.163]