Figure 6.11 Stress vs. strain at various temperatures for BASF Ultramid B3EG5—stabilized, 25% glass fiber reinforced Nylon 6 resin (DAM). Figure 6.11 Stress vs. strain at various temperatures for BASF Ultramid B3EG5—stabilized, 25% glass fiber reinforced Nylon 6 resin (DAM).
Figure 6.152 Dielectric strength vs. moisture content and temperature for BASF Ultramid A3EG6—30% glass fiber, heat stabilized Nylon 66 resin [8]. Figure 6.152 Dielectric strength vs. moisture content and temperature for BASF Ultramid A3EG6—30% glass fiber, heat stabilized Nylon 66 resin [8].
Figure 6.156 Volume resistivity vs. temperature and various moisture levels for BASF Ultramid A3EG6—high stiffness, 30% glass fiber filled Nylon 66 resin [8]. Figure 6.156 Volume resistivity vs. temperature and various moisture levels for BASF Ultramid A3EG6—high stiffness, 30% glass fiber filled Nylon 66 resin [8].

See other pages where Nylon BASF Ultramid glass fiber is mentioned: [Pg.64]   
See also in sourсe #XX -- [ Pg.201 ]




SEARCH



BASF

Fiber glass fibers

Glass fiber/nylon

Glass fibers

Nylon BASF Ultramid

Nylon fibers

UltraMide

© 2024 chempedia.info