The catalyst was prepared by impregnation of the powdered activated carbon support, Norit SX Ultra, (surface area 1200 m g ) with sufficient palladium nitrate to produce a metal loading of 3 %. The resulting suspension was dried and calcined at 423 K for 3 hours. The dispersion of the catalyst was... [Pg.174]

Norit SX ULTRA 1200 Acid washed steam activated carbon 9.0... [Pg.49]

Further studies by the same group involved mainly CoTAA and also CoTMPP. These molecules were adsorbed on Norit SX Ultra and were usually pyrolyzed between 600 and 800°C. The optimum CoTAA loading was 13 wt% chelate ( 2.3 wt% Co). At the lowest heat-treatment temperature (600°C), the... [Pg.94]

Figure 2. Cobalt buttons produced from cobalt sulfate prepared using C0SO4 from Alfa Asear (a) without activated carbon treatment (3 hours of deposition) and (b) treated with 4 g/L Norit SX-Ultra activated carbon (6 hours of deposition)... Figure 2. Cobalt buttons produced from cobalt sulfate prepared using C0SO4 from Alfa Asear (a) without activated carbon treatment (3 hours of deposition) and (b) treated with 4 g/L Norit SX-Ultra activated carbon (6 hours of deposition)...
TpOCHsPPCo, TpCFsPPCo, CoTAA Printex XE2 carbon black Norit SX ultra active charcoal 500-800 2h N2, Ar 800 PEMFC [72]... [Pg.16]

CoTAA Norit SX Ultra active charcoal 500-900 2h Ar 800 0.25 M H2SO4 [73]... [Pg.17]