Nonweathered coatings, photoinitiation rate

Photoinitiation Rate Measurements on Model Systems and Nonweathered Coatings... [Pg.265]

Fig. 11. Gloss loss rate in unstabilized acrylic melamine coatings versus the square root of the nonweathered photoinitiation rate of those coatings. Coatings were exposed to harsh exposure conditions. Fig. 11. Gloss loss rate in unstabilized acrylic melamine coatings versus the square root of the nonweathered photoinitiation rate of those coatings. Coatings were exposed to harsh exposure conditions.

See other pages where Nonweathered coatings, photoinitiation rate is mentioned: [Pg.269]    [Pg.269]    [Pg.263]    [Pg.267]    [Pg.269]    [Pg.270]    [Pg.271]    [Pg.269]   