Microstructure zirconia-toughened alumina

Properties of zirconia toughened alumina, ZTA, depend on the specific microstructure and the proportions of zirconia and alumina. To convert MPa to psi, multiply by 145. [Pg.325]

Figure 1.5 Microstructure of a zirconia-toughened alumina back-scattered electron image using the SEM. The bright phase is zirconia. Figure 1.5 Microstructure of a zirconia-toughened alumina back-scattered electron image using the SEM. The bright phase is zirconia.
Controlled or graded microstructures, for example, zirconia toughened alumina (ZTA), can be made by depositing a Zr02 slurry onto an AI2O3 substrate (Gebhardt 2006). [Pg.1028]

FIGURE 6.11 Chemical composition (A) and microstructure (B) of zirconia-toughened alumina composite, BIOLOX Delta (provided courtesy of CeramTec AG, Plochingen, Germany). [Pg.65]


See other pages where Microstructure zirconia-toughened alumina is mentioned: [Pg.105]    [Pg.105]    [Pg.12]    [Pg.442]    [Pg.672]    [Pg.381]    [Pg.513]    [Pg.442]    [Pg.391]    [Pg.410]    [Pg.91]    [Pg.167]    [Pg.325]    [Pg.325]    [Pg.7]    [Pg.94]    [Pg.310]    [Pg.65]    [Pg.333]    [Pg.514]   
See also in sourсe #XX -- [ Pg.254 ]