Glass-ceramic matrix composites with oxide fibers

As mentioned previously, one of the major concerns for glass-ceramics reinforced with continuous fibers is the effect of matrix cracks in oxidizing environments. An important parameter in this kind of composite is the... [Pg.294]


See other pages where Glass-ceramic matrix composites with oxide fibers is mentioned: [Pg.280]    [Pg.293]    [Pg.292]    [Pg.385]    [Pg.103]    [Pg.4]    [Pg.17]    [Pg.508]    [Pg.218]    [Pg.292]    [Pg.120]    [Pg.141]    [Pg.315]    [Pg.279]    [Pg.147]    [Pg.261]    [Pg.599]    [Pg.1555]    [Pg.390]    [Pg.6]    [Pg.202]    [Pg.101]    [Pg.436]    [Pg.456]    [Pg.169]   
See also in sourсe #XX -- [ Pg.467 ]




SEARCH



Ceramer composites

Ceramic compositions

Ceramic fibers

Ceramic matrix composite

Ceramic-matrix

Ceramics ceramic-matrix composites

Ceramics) composites

Composite glass fiber

Composite matrices

Fiber glass fibers

Glass compositions

Glass fibers

Glass fibers composition

Glass matrix

Glass-ceramics composition

Glass/ceramic composite

Glasses glass ceramics

Matrix composition

Matrix fibers

Oxidation ceramics

Oxide fibers glass matrix composites

Oxide glass

Oxide matrices

© 2024 chempedia.info