Big Chemical Encyclopedia

Chemical substances, components, reactions, process design ...

Articles Figures Tables About

Electrode burn-off

Figure 6.156 Copper electrode burn-off versus arcing time t for short-circuit currents in the range 0.8kA. ..15kA rms. Figure 6.156 Copper electrode burn-off versus arcing time t for short-circuit currents in the range 0.8kA. ..15kA rms.
For copper, the electrode burn-off versus arcing time has been measured for different short-circuit currents up to 15 kA (root mean square value), see Fig. 6.156. [Pg.317]

Electrode Energy content of electrode burn-off Oxidation heat... [Pg.320]

Figure 6.160 Particle-induced flame transmission, caused by aluminium electrode burn-off. Gap w versus arc peak power Nz at the moment of flame transmission. Aluminium electrodes ... Figure 6.160 Particle-induced flame transmission, caused by aluminium electrode burn-off. Gap w versus arc peak power Nz at the moment of flame transmission. Aluminium electrodes ...