Ekkcel 1-2000, aromatic polyesters

The tensile strength of this copolymer (EKKCEL 1-2000) is 14,000 psi at room temperature, and 3,000 psi at 500°F. Its heat deflection temperature is 560°F, and the upper use temperature for the polymer will probably be in the range of —575°F. The water absorption is extremely low for this material, as it is for all the aromatic polyesters described here. [Pg.160]

In 1972, Cottis and coworkers at Carborundum patented wholly aromatic polyesters based on p-hydroxybenzoic acid (HBA), A,A -dihydrox-ybiphenyl (DHB), and terephthalic acid (TPA), one of which was later commercialized as EKKCEL 1-2000 [1]. In 1974, Kuhfuss and coworkers at Eastman Kodak reported a new polyester based on HBA and polyfethylene terephthalate) (PET), which was later marketed under the code of X-7G. X-7G is the first thermotropic liquid crystalline polymer to be fabricated by injection molding or melt spinning [2]. However, then Eastman Kodak withdrew its plan of marketing of X-7G and changed the target with a wholly aromatic polyester commercialized as TITAN (THERMX ) in 1996. As described later, it was acquired by DuPont in 2003. [Pg.239]

MELT PRXESSABLE WHOLLY AROMATIC POLYESTER -EKKCEL 1-2000 (CARBORUNDUM)... [Pg.236]


See other pages where Ekkcel 1-2000, aromatic polyesters is mentioned: [Pg.2298]    [Pg.187]    [Pg.609]    [Pg.187]    [Pg.609]    [Pg.36]    [Pg.187]    [Pg.609]    [Pg.237]    [Pg.13]    [Pg.4260]    [Pg.160]   
See also in sourсe #XX -- [ Pg.3 , Pg.10 ]

See also in sourсe #XX -- [ Pg.3 , Pg.10 ]




SEARCH



Aromatic polyester

Ekkcel

© 2024 chempedia.info