Big Chemical Encyclopedia

Chemical substances, components, reactions, process design ...

Articles Figures Tables About

Bashore rebound

The stress at 50X compression, tensile properties, and Bashore rebound were measured according to ASTM D-3574, Section C, E, and H, respectlyely. [Pg.267]

Polyurethane elastomers with higher hard segment content result in more hard segments mixed into the soft phase [25-27]. Also, polyester soft segments are more compatible with urethane hard segments. The decrease in Bashore rebound values of TG-225, TG-250 and TG-275 extended materials is associated with the lower degrees of phase... [Pg.403]


See other pages where Bashore rebound is mentioned: [Pg.247]    [Pg.427]    [Pg.430]    [Pg.526]    [Pg.527]    [Pg.528]    [Pg.529]    [Pg.530]    [Pg.538]    [Pg.539]    [Pg.540]    [Pg.543]    [Pg.546]    [Pg.547]    [Pg.549]    [Pg.550]    [Pg.373]    [Pg.377]    [Pg.391]    [Pg.402]    [Pg.10]    [Pg.337]    [Pg.337]    [Pg.337]    [Pg.338]   
See also in sourсe #XX -- [ Pg.373 ]




SEARCH



Rebound

Rebounding

© 2024 chempedia.info