In a similar multiphase system, transition metal carbides were used as additives for pressureless sintering of TiB2, yielding composites of binary and ternary borides [218,296]. Attrition milled powder mixtures of TiB2 with 3-10 mass-% Co or Ni and 20-35 mass-% WC have been sintered in a vacuum at temperatures between... [Pg.916]