SEARCH Articles Figures Tables DSC of miciocryslalline, paraffinic, and Fischer-Tropsch waxes on the reheat cycle. Samples were first heated to 175 C, then cooled to —50 C, followed by reheating to 175 C, all at 20 C min. Heat of fusion for each is shown in the legend. [Publishers Imprint] [Publishers Imprint]